Surface roughness improved to Ra 0.4 on Inconel parts.

Aerospace Component Surface Finish Upgrade

The problem

Heat resistant alloy components were meeting dimensional tolerance but failing surface roughness requirements on curved surfaces.

  • Surface roughness above specification on curved faces
  • Heat build-up at the cutting edge
  • Short tool life in heat resistant alloy

What we changed

A ball nose geometry with a matched coating was selected and step-over was recalculated to keep scallop height inside the requirement.

The result

Surface roughness met the requirement and the operation no longer needed a separate polishing step.

Application data can be shared under agreement.

← Back to Cases

Need a quotation or technical advice?

Send us your drawing, grade requirement or application details. Our engineers reply within one working day.

Get a Quote